Choosing a UV Printer?

How to Test UV Ink Adhesion on Medals, Coins and Buttons

Print bigger, print faster — wide-format UV flatbed printers for signs, decor and industrial work.

How to Test UV Ink Adhesion on Medals, Coins and Buttons
Posted on by John White

Qualify UV ink adhesion on medals, coins and buttons with the exact blank construction, coating and production recipe. A generic “metal” result is not enough: plating, paint, lacquer, protective film, casting residue and supplier changes can alter the surface. Test a controlled matrix, allow the agreed conditioning time, and judge appearance plus the handling stresses required by the order.

  • Identify substrate, finish, supplier and lot before cleaning.
  • Keep one untreated control and change only one variable per comparison.
  • Record ink/layer recipe, cure condition and test timing.
  • Do not turn a tape result into a universal durability claim.

The medals, coins and buttons printer collection covers application selection. This supporting article owns surface qualification.

Define what the test must prove

Specify whether the printed item will be decorative, carried in a pocket, rubbed, cleaned, packaged face-to-face or used outdoors. Define acceptable visual change and whether the test is destructive. Keep production acceptance separate from exploratory testing so operators do not damage sellable goods.

Identify and prepare representative blanks

Record base material when known, plating/coating, color, texture, supplier code and lot. Photograph both faces and retain an unprinted blank. Remove protective film and inspect for oil, oxidation, polishing compound or handling marks. Use only a cleaning method compatible with the finish.

Mimaki's UV ink adhesion guidance notes that surface and pretreatment strongly affect adhesion and specifically discusses primer for inorganic surfaces such as metal. It supports the need for testing; it does not prove that any specific primer or AndresJet setting will suit a customer's finish.

Build the smallest useful test matrix

Sample Variable Everything held constant
A Untreated control Blank lot, artwork, layers, mode and cure
B Qualified cleaning method Same as A
C Candidate pretreatment, if justified Same as A
D One cure or layer change, if justified Preparation fixed to best prior result

Do not compare five changes at once. If sample C performs better, the record must show whether only pretreatment changed. Print representative solids, fine text, edges and white/color overlaps because failure can depend on ink build and location.

Condition before rating

Record elapsed time, temperature range and handling before testing. Use the same schedule for every sample. For an internal tape or cross-cut screen, define the tape, cut pattern, removal direction and rating photographs. Treat it as a comparative production method unless the company follows a named standard exactly with trained operators and appropriate equipment.

ASTM D3359 is often mentioned for coatings, but its scope and limitations matter; because the standard page could not be reliably reopened during this review, it is deliberately not linked or claimed as the executed method here. This prevents a standard name from overstating an informal shop-floor check.

Add end-use checks beyond initial adhesion

Inspect after pocket abrasion, stacking, wiping or another customer-agreed simulation. Check edges and raised details, not only the center. If a clear layer is used, test the complete stack. Approval should state exactly what passed, for example “supplier lot X, cleaned by method Y, recipe Z, passed the agreed tape screen after the stated conditioning period.”

Release a repeatable recipe

Record Required detail
Blank Supplier, code, construction, finish and lot
Preparation Cleaner/pretreatment, method and operator
Print File revision, layers, mode and fixture
Conditioning Time and environment
Evaluation Method, photos, result and approver
Boundary Approved uses and requalification triggers

Requalify when supplier, plating, coating, lot, cleaner, primer, ink, layer build, cure condition or end use changes. The AJ1206 page can support a sample-print discussion, but final suitability comes from the recorded test on the submitted blanks.

Distinguish adhesion loss from ink-film damage

Record where separation occurs. Ink lifting cleanly from the blank suggests an interface problem; separation between printed layers suggests a layer or cure interaction; cracking without lift may mean that a rigid film was stressed. Photograph the failure under consistent light and mark its location before discarding the test piece.

Test the center, edge, recessed detail and any area with a different ink build. A good result on a flat center does not represent an embossed rim. If a button shell will be formed or assembled after printing, evaluate the completed process because deformation may expose a failure absent on the flat component.

Set sampling and decision rules before production

The plan should state which lots, finishes and representative pieces are included, how many repetitions are needed and who approves. Keep sacrificial blanks or coupons for destructive checks. Production inspection can then monitor the approved attributes without damaging sellable pieces.

Use three clear outcomes: pass and release; fail and reject; or hold for additional controlled testing. Avoid a conditional pass without written restrictions. If testing covered indoor decorative handling only, the result cannot support claims about outdoor exposure, dishwashing, chemicals or indefinite abrasion resistance.

Close a failed qualification methodically

Preserve the failed sample and untreated control. Confirm that preparation, artwork, layers, conditioning time and evaluation method matched the plan. Change one suspected variable, repeat the comparison and check for new appearance or handling problems. A correction is ready only when its result repeats and the revised recipe states exactly which blank construction and use it covers.

Evidence to retain for repeat orders

Keep the approved blank, material and supplier identification, photographs of preparation and loading, released artwork, fixture or bed-position record, machine condition checks, first-article measurements, inspection results and corrective actions. Evidence should let a different trained operator reproduce the decision without relying on memory.

Requalification is triggered by a changed supplier, lot, coating, dimensions, artwork geometry, layer build, ink or pretreatment, fixture, machine condition, acceptance criterion or intended use. If the team cannot confirm that controlled inputs remain equivalent, run a new representative sample. This is also the right point to tell the customer which claim has been verified and which performance remains outside the evidence.

For an equipment inquiry, supply the blanks, layered files, expected order mix, tolerances, end-use stresses and rejected examples. Ask for the demonstration to reproduce the real loading and inspection route. A visually attractive isolated sample is useful, but it does not establish batch repeatability, accepted output or durability outside the stated test.

For the complete decision path, continue with the uv curing, adhesion & durability guide.

Frequently asked questions

Does every metal blank need primer?

No. Test the exact surface without and with justified preparation; primer may change appearance or process time.

Is a scratch test enough?

No single check represents every use. Pair adhesion screening with the handling, cleaning or abrasion risk defined by the buyer.

Can a passed recipe be reused next year?

Only after confirming that all controlled inputs remain equivalent and a new first article passes.

Latest Stories

This section doesn’t currently include any content. Add content to this section using the sidebar.